The structure was mechanically cleaned with subsequent degreasing of the surface, then zinc-coated with the composition of GALVANOL using a brush.
8 (800) 222-39-73
Горячая линия по вопросам Цинкирования
Расположение объекта
AlexandrovДата нанесения состава
Restoration of the lost coating on the ship’s hull was performed by applying the composition with a brush and spray gun.