The total thickness of the self-coating was 80-100 microns.
8 (800) 222-37-63
Горячая линия по вопросам Цинкирования
The total thickness of the self-coating was 80-100 microns.
The composition was applied as a primer in two layers with a total thickness of 80 microns, after which a two-component polyurethane finish coating was applied in one layer.
The composition was applied in two layers with a total thickness of 80 microns.