Fan grilles
Application of a coating with a total thickness of at least 80 microns.
8 (800) 222-37-63
Горячая линия по вопросам Цинкирования
Application of a coating with a total thickness of at least 80 microns.
Applying a zinc coating in 2 layers.
Application of GALVANOL with a total thickness of at least 80 microns to the prepared surface, followed by application of 40 microns of ALINOL.
ALINOL was used as a decorative coating. The total thickness of the protective coatings was about 100 microns.
The protective coating was applied in several layers, with a total thickness of at least 100 microns, on mechanically prepared and degreased metal. The application process was carried out with a spray gun and brush. Also, during the installation of the system, THE galvanol composition protected the welds.
Application of the zinc coating composition in 2 layers with a total thickness of at least 80 microns.
Preparation of metal for painting were produced by mechanical means (kvartsevanie), followed by degreasing. The composition of GALVANOL was applied to the prepared surface using a spray gun and rollers in 2 layers.
Restoration of the lost coating on the ship’s hull was performed by applying the composition with a brush and spray gun.
Application of the composition by air in 2 layers.
The composition of GALVANOL was applied with an airless spray gun on a cleaned and degreased surface.
The zinc composition is applied by airless spraying on the surface prepared by mechanical means, with degreasing, in 2 layers.
Preparation of metal by mechanical means, applying the composition by air spray in 2 layers.